Five properties of PVC edge banding strips

Release time:

2024-02-02

The content of calcium carbonate powder (commonly known as lime powder) in PVC edge banding strips. Generally, PVC edge strips contain calcium carbonate powder, but too high a content of calcium carbonate powder will cause the structure of PVC to become loose, thus seriously affecting the quality of PVC edge strips. Problems caused by excessive calcium carbonate powder content include:

1) Whitening, that is, after the PVC edge banding strip is bent in a small arc, whitening will appear in the edge part, and this whitening will not recover after the PVC edge banding strip is straightened again. This phenomenon will be more obvious for dark colors.

2) Jumping edges, which are easy to occur when trimming PVC edge banding strips. Of course, the cause of edge jumping is not only the excessive content of calcium carbonate powder. When doing edge banding, when the hot melt adhesive for edge banding and the feeding speed are not well coordinated, it will cause the PVC edge banding strip to not be completely bonded to the board during edge trimming. Therefore, due to the PVC edge banding strip The floating phenomenon is prone to edge jumping.

3) The edge gloss of the PVC edge strip after trimming and grinding will be poor, so the appearance will be poor. In order to reduce costs, the inferior PVC edge banding strips currently on the market contain calcium carbonate powder content as high as 60% or more. As for different equivalent products of the same brand, the main reason is their calcium carbonate powder content.

4) Cracking. Due to the high content of calcium carbonate, the PVC edge banding strip has no toughness and a loose internal structure. It will crack under slight external force, especially during transportation at low temperatures.

PVC cannot be directly bonded to the board. The quality of the adhesive (actually not glue, but acts as a bridge, so it is also called a bridging agent) directly affects the bonding effect. Especially when the weather is cold, the workshop temperature is relatively low, and the efficiency of hot melt adhesive and back glue is greatly reduced. This is a reason that furniture manufacturers often blame on the quality of PVC edge strips. The best way to deal with it is to replace it with high-temperature hot-melt adhesive with higher viscosity and purity, increase the working temperature of the hot-melt adhesive, raise the room temperature, and preheat the PVC edge banding strip (quality must be guaranteed).

The curvature of the PVC edge strip itself. In order to prevent the loss of glue when the PVC edge strip is bonded and extruded, a good PVC edge strip should have a slight inward bend in its width direction. Inferior PVC edge strips are flat or even warped, making them prone to poor bonding.

Currently, there are only a few PVC edge strips on the market that are acrylic products. While others are transparent PVC. The problem with transparent PVC is that after trimming and grinding, its edges will become slightly less transparent, so the 3D effect cannot be fully achieved.

PVC surface printing patterns There are two processes for PVC surface: printing and heat transfer film. The surface of thermal transfer film is relatively shiny, and the product looks bright and layered. However, due to its high cost, slow transfer speed, and inability to easily match the color to the board, it has now been replaced by printing. The calcium carbonate powder content of some inferior PVC edge banding strips is too high. If the printing process is used, there will be a color fading problem, so sometimes the heat transfer film process is used.